Hobart® MaxalTig® 4943

Alloy 4943 filler metal was formulated to be welded with the same weld procedure specifications as 4043 and 4643, and does not depend upon dilution from the base metal during welding to increase the strength of the weld deposit, while maintaining the same weld characteristics and benefits of 4043 and 4643.
Features/Benefits:
- Moderate/high strength (33 ksi typical)
- Low melting temperature/high fluidity
- Low welding smut and discoloration
- Low ductility, formability, and lower toughness (similar to 4043)
- Moderate electrical conductivity and thermal conductivity
- Post weld fully heat treatable requiring no base metal dilution
- Excellent corrosion resistance
- Low shrinkage rate/reduced distortion
- Low hot cracking sensitivity in most applications

FLAT/HORIZONTALFLAT/HORIZONTALFLAT/HORIZONTALOVERHEADVERTICAL UPVERTICAL DOWN

AWS: A5.10: ER4943, R4943

Data Sheet: English, French

SDS: English (NA), Spanish (NA), French (NA)

Certification: Download PDF

Approvals: ABS, CE, CWB

Product Sizes & Specifications

Part Number Diameter (IN) Diameter (MM) Package Base Metal Welding Process Welding Position
494309470 3/32 2.4 10 Lb (4.5 Kg) Carton aluminum GTAW (TIG) all
494312570 1/8 3.2 10 Lb (4.5 Kg) Carton aluminum GTAW (TIG) all
494315670 5/32 4 10 Lb (4.5 Kg) Carton aluminum GTAW (TIG) all

Applications

Welding 6xxx alloys, radiators and air conditioning components, general repair and maintenance, water and gas tight applications, post weld age, post weld heat treat & age applications, automotive/motorcycle frames, sports products - scooters/bicycles, general repair and maintenance, aerospace hardware, ladders and frames, alloy 356 castings, wheels, ship decks, furniture

Similar Products

  • Hobart® MaxalTig® 4043

    Hobart® MaxalTig® 4043

    4043 filler metal is a popular aluminum/silicon filler alloy for general purpose welding applications. Features/Benefits: - Moderate strength (27 ksi typical) - Low melting temperature/high fluidity - Low welding smut and discoloration - Low ductility, formability, and lower toughness - Moderate electrical conductivity and thermal conductivity - Excellent corrosion resistance - Low shrinkage rate/reduced distortion - Low hot cracking sensitivity in most applications

    View Details

    Where To Buy

  • Hobart® MaxalTig® 5356

    Hobart® MaxalTig® 5356

    5356 filler metal is the most common aluminum/magnesium alloy for general purpose welding and is typically used in the construction industry in fabricating truck trailers, small fishing boats, and in cryogenic applications. Features/Benefits: - High strength (40 ksi typical) - High ductility/fatigue strength/very high toughness - Moderate ductility/formability - Lower electrical conductivity and thermal conductivity - Higher column strength/better feedability - Very good color match after anodizing with 5xxx/6xxx base materials

    View Details

    Where To Buy